Carbon Black |
Standard |
N110 |
N115 |
N121 |
N134 |
N219 |
N220 |
|
||||||
Item |
||||||
Ioding AdsorptionNumber g/kg |
145±8 |
160±8 |
121±7 |
142±8 |
118±7 |
121±7 |
DBP Absorption Number 10-5M3/kg |
113±7 |
113±7 |
132±8 |
127±7 |
78±7 |
114±7 |
DBP Compressed Sample10-5M3/kg |
89-105 |
89-105 |
103-119 |
95-111 |
67-91 |
90-106 |
CTAB surface Area103M2/kg |
117-135 |
119-137 |
112-130 |
124-144 |
98-116 |
102-120 |
Nitrogen Surface Area103M2/kg |
120-134 |
129-145 |
115-129 |
135-151 |
109-123 |
112-126 |
Tint Strength % |
115-131 |
115-131 |
111-127 |
123-139 |
115-131 |
108-124 |
Heating Loss %≤ |
3 |
3 |
3 |
3 |
2.5 |
2.5 |
Ash Content % |
0.7 |
0.7 |
0.7 |
0.7 |
0.7 |
0.7 |
45μm Sieve Residue % ≤ |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
500μm Sieve Residue % ≤ |
0.001 |
0.001 |
0.001 |
0.001 |
0.001 |
0.001 |
Impurity |
no |
no |
no |
no |
no |
no |
stress at 300% Elongation Mpa |
-3.5±1.6 |
-3.4±1.6 |
-0.4±1.6 |
-1.8±1.6 |
-3.9±1.6 |
-2.3±1.6 |
Characteristics of vulcanized rubber |
N110: High reinforcing, super abrasion |
|||||
N115: High reinforcing, super abrasion |
||||||
N121: High reinforcing, super abrasion, high modulus |
||||||
N134: High reinforcing |
||||||
N219: High reinforcing, low modulus, good elongation and resistance to tearing, good flex resistance |
||||||
N220: High reinforcing, high tear resistance, good processing |
||||||
Standard |
N375 |
N539 |
N550 |
N660 |
N762 |
N774 |
|
||||||
Item |
||||||
Iodine Adsorption Number g/kg |
90±7 |
43±6 |
43±6 |
36±6 |
27±6 |
29±6 |
DBP Absorption Number 10-5M3/kg |
114±7 |
111±7 |
121±7 |
90±7 |
65±6 |
72±7 |
DBP Compressed Sample10-5M3/kg |
88-104 |
73-89 |
77-93 |
66-82 |
53-65 |
57-69 |
CTAB surface Area103M2/kg |
87-105 |
34-48 |
35-49 |
29-43 |
23-35 |
23-35 |
Nitrogen Surface Area103M2/kg |
86-100 |
33-45 |
34-46 |
29-41 |
24-34 |
25-35 |
Tint Strength % |
106-122 |
- |
- |
- |
- |
- |
Heating Loss %≤ |
2.5 |
1.5 |
1.5 |
1.5 |
1.5 |
1.5 |
Ash Content % |
0.7 |
0.7 |
0.7 |
0.7 |
0.7 |
0.7 |
45μm Sieve Residue % ≤ |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
500μm Sieve Residue % ≤ |
0.001 |
0.001 |
0.001 |
0.001 |
0.001 |
0.001 |
Impurity |
no |
no |
no |
no |
no |
no |
stress at 300% Elongation Mpa |
0.1±1.6 |
-1.6±1.6 |
-0.9±1.6 |
-2.6±1.6 |
-4.9±1.6 |
-4.1±1.6 |
Characteristics of vulcanized rubber |
N375: medium-high reinforcing, high modules and hardness, smooth surface of extrusion |
|||||
N539: Medium-high reinforcing, high modulus and hardness, smooth surface of extrusion |
||||||
N550: Medium-high reinforcing, high modulus and hardness, smooth surface of extrusion |
||||||
N660: medium-high reinforcing and modulus, good flex resistance, low heat buildup |
||||||
N762: low reinforcing |
||||||
N774: semi-reinforcing, good elongation, high resilience, low compressed deformation |
||||||
Standard |
N234 |
N326 |
N330 |
N339 |
N347 |
N351 |
|
||||||
|
||||||
|
||||||
Item |
||||||
Coding Adsorption Number g/kg |
120±7 |
82±7 |
82±7 |
90±7 |
90±7 |
68±7 |
DBP Absorption Number 10-5M3/kg |
125±7 |
72±7 |
102±7 |
120±7 |
124±7 |
120±7 |
DBP Compressed Sample10-5M3/kg |
94-110 |
62-74 |
80-96 |
91-107 |
91-107 |
87-103 |
CTAB surface Area103M2/kg |
110-128 |
74-92 |
73-91 |
84-102 |
78-96 |
64-82 |
Nitrogen Surface Area103M2/kg |
112-126 |
71-85 |
71-85 |
84-98 |
78-92 |
64-78 |
Tint Strength % |
115-131 |
103-119 |
96-112 |
103-119 |
97-113 |
92-108 |
Heating Loss %≤ |
2.5 |
2.5 |
2.5 |
2.5 |
2.5 |
2.5 |
Ash Content % |
0.7 |
0.7 |
0.7 |
0.7 |
0.7 |
0.7 |
45μm Sieve Residue % ≤ |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
500μm Sieve Residue % ≤ |
0.001 |
0.001 |
0.001 |
0.001 |
0.001 |
0.001 |
Impurity |
no |
no |
no |
no |
no |
no |
stress at 300% Elongation Mpa |
-0.4±1.6 |
-3.9±1.6 |
-0.9±1.6 |
0.6±1.6 |
0.2±1.6 |
0.8±1.6 |
Characteristics of vulcanized rubber |
N234: High reinforcing, high abrasion, high modulus, good dispersion |
|||||
N326: Medium-high reinforcing, low modules, good elongation and resistance to tearing, good flex resistance |
||||||
N330: medium-high reinforcing and modulus, good processing |
||||||
N339: medium-high reinforcing, high modulus and hardness, good processing |
||||||
N347: medium-high reinforcing, high modulus and hardness, good processing |
||||||
N351: medium-high reinforcing, high modulus and hardness, good processing |
Packing of Carbon Black
20kg/package: 1MT/Pallet
1000kg/package: 1MT/Pallet
Or customized
Application of Carbon Black
Carbon black is mainly used as reinforcing filler in tyres and other rubber products during the vulcanization process to improve the tensile strength and wear resistance of styrene-butadiene, such as rubber conveyor belts, rubber hose, Airsprings and other rubber chemicals.
As one of carbon black suppliers, we can provide high quality carbon black N220, carbon black N330, carbon black N660 for sale, if you have needs, please contact us.
If you are looking for a reliable rubber raw material manufacturer, please choose us, and we will be your best partner.
Buen trato: comprar del vendedor
Esta página es acerca de los importadores y exportadores de Carbon Black Buscar en la categoria : Varios / Descuento Buscar en la categoria : carbon, black |
Sábado 30 julio 2016
Precio : 3 200,00 €
A digitally controlled servomotor, curve smoothing function and 32-bit RISC CPU provide exacting high-speed cutting, with a maximum cutting speed of 33 in/sec. Three standard cutting modes - normal, heavy and high - provide optimum versatility. For utmost agility and precision, the...
Jueves 01 septiembre 2011
100% pure Argan soap, Excellent for dry or sensitive skin. Naturally high in unsaturated fatty acids, oleic and linoleic acids and Vitamin E.Great slightly nutty natural scent. *Price : 0.9 - 1.6 Euro/100grs , MOQ 1200 pieces (100kg)Ubicación : Soc 16 Derb Bennis, Fès médina, Fez...
Jueves 15 enero 2009
Desiccated Coconut Desiccated coconut high fat fine and mediumg grades: - Moisture: 3% max, - FFA: 0.3 % max, - Oil content: 62% min, - Free from ecoli or bactereia, no foreign matterUbicación : 20/5 Dinh Bo Linh str Binh Thanh Distr, 84 Ho Chi Minh, Persona a contactar : Smith Nguyen...