Molybdenum strip with CMTR ASTM B386-91 Mo1 99.95% rolling bright
|
Item name |
Molybdenum circle |
Standard |
ASTM B386-91 |
Specification |
as requriment |
Thickness |
0.05-50.0mm |
Diameter |
Max350mm |
purity |
99.95% |
Surface |
Black / bright / pickling / alikaline |
Processing |
Drawing |
Classify |
Mo1, TZM,(Mo-Ti-Zr alloy) |
MOQ |
1pc |
Feature:
1. With high temperature resistance, low pollution
2. High purity, good plasticity
3. TZM has a higher recrystallization temperature, higher creep strength and higher tensi le strength than pure molybdenum
Application
1. Suitable for producing ion implantation parts
2. For producing electric light source parts, components of electric vacuum and electric power semiconductor
3. For producing Mo-boat, heat shield and heat bodies in high temperature furnace< /p>
Chemical component
Grade |
% impurity content % max |
||||||||
Fe |
Ni |
Al |
Ca |
Si |
Mg |
C |
N |
O |
|
Mo-1 |
0.010 |
0.005 |
0.002 |
0.002 |
0.01 |
0.002 |
0.01 |
0.003 |
0.008 |
Buen trato: comprar del vendedor
Esta página es acerca de los importadores y exportadores de Molybdenum strip with CMTR ASTM B386-91 Mo1 99.95% rolling bright Buscar en la categoria : Varios / Descuento Buscar en la categoria : b386, rolling, strip, with, molybdenum, astm, cmtr |
Jueves 30 junio 2022
What is Stainless Steel 304 Seamless Pipe ? Stainless Steel 304 seamless pipe is one of the most cost-effective and regularly utilised grades which is available in the market. The Schedule 10 SS 304 Pipe has great corrosion resistance and they show outstanding oxidation resistance...
Sábado 19 diciembre 2020
Cantidad : 1 - Precio : $ 640
Genuine Printhead XAAR 500/80pl To be used with: MYJET LA3208XR,MYJET LA3204XR, MYJET LB3204XR, MYJET LB3208XR, MYJET WD3212XR, MYJET WD3216XR, LIYU PE3204-XR382, LIYU PE3208-XR382, SMART PROTON 8H, Wit-color Ultra2000 H4/H6, WIT-COLOR ULTRA2000 H8, WIT-COLOR ULTRA2000 H12, WIT-COLOR...
Sábado 10 septiembre 2022
Small graphite crucible works best with a quartz jacket because graphite oxidizes. high purity graphite crucible is good or bad with its material and density. Good graphite crucible doesn't oxidizes easily, so that the production loss is low. Bad graphite oxidation is not uniform...