Model | Hardness | Tensile strength | Extension elongation | Flame Rating-UL94 | Proportion |
GE-370A | 70A | 9.8 | 780 | 0.95 | |
GE-375A | 75A | 7.8 | 750 | 0.97 | |
GE-380A | 80A | 4.6 | 220 | 94V0 | 1.05 |
GE-385A | 85A | 10 | 550 | VW-1 | 1.08 |
GE-388A | 88A | 6 | 500 | 94V0 | 1.05 |
GE-392A | 92A | 10 | 650 | 0.965 | |
All the raw materials are from USA-KRATON, Japan-KURARAY, Taiwan, Korea-SK and so on.
Thermoplastic Elastomer(TPE) is an injection-molding material which has the characteristics of high elasticity, high strength, high elastic resilience.
Advantages: non-toxic, eco-friendly, wide range of hardness, excellent processing, no vulcanization.TPE not only can conduct second injection molding with PP,PE,PC,PS,ABS and so on, but also can separate molding
Before or after using this product, please clean it thoroughly with PE or PP(MI:0.5~2.5).
Do not need to de dry in normal condition, de dry for two hours when TPE was stored for a long time
Using high melt index color concentrate can receive a better result
Advise to use 3% color concentrate
Clients should test it to decide if the color concentrate can be used
Buen trato: comprar del vendedor
Esta página es acerca de los importadores y exportadores de Inflaming Retarding Thermoplastic Elastomer for Wire and cable Buscar en la categoria : Materias primeras Buscar en la categoria : elastomer, retarding, cable, thermoplastic, wire, inflaming |
Viernes 01 julio 2022
Cantidad : 300
Câble HDMI ethernet 3D pour télé plasma et LCD. Améliorez la qualité de votre système cinéma! Les télés LCD et à écran plasma 3D ont besoin de câble de très haute qualité. Les câbles HDMI de Reekin permettent de pousser au maximum la capacité de votre système cinéma. Ils sont également...
Sábado 16 marzo 2024
cylindrical graphite crucible works best with a quartz jacket because graphite oxidizes. High purity graphite crucible is good or bad with its material and density. Good graphite crucible doesn't oxidizes easily, so that the production loss is low. Bad graphite oxidation is not uniform...
Jueves 25 octubre 2018
Cantidad : 35 racks - Precio : 60 E piece
Rack de stockage à glissiéres Prof 150cm Larg 100cm Hauteur 100cm 40 piéces - trés bon état Ubicación : 51 rue léonard de Vinci, 62730 Marck, Persona a contactar : vincent Delattre, 03 21 96 98 22